Sendust Cores DM Inductor
1、Lower core loss than Iron Powder.2、Low magnetostriction coefficient, low audible noise.3、Good temperature stability. Under 4% from -15 'C to 125 'C4、Maximum flux density: 10,000 gauss (1.0 tesla)5、Inductance tolerance: 8%.